Труды сотрудников института физики

w10=
Найдено документов в текущей БД: 11

    Magnetic characteristics of primary concentrates supplied as a feedstock to Abagur enrichment-agglomeration plant
/ E. K Yakubailik [et al.] // J. Min. Sci. - 2013. - Vol. 49, № 1. - P. 153-159, DOI 10.1134/S1062739149010188. - Cited References: 7 . - ISSN 1062-7391
РУБ Mining & Mineral Processing

Кл.слова (ненормированные):
primary concentrate -- magnetite ore -- lightly-oxidized ore -- magnetic properties

Аннотация: The article presents basic magnetic characteristics of nine primary concentrates produced from Siberian magnetite ore and a lightly oxidized iron ore and supplied as a feedstock to Abagur enrichment-agglomeration plant. The best magnetic properties belong to the primary concentrate produced from the magnetite ore mined at Abaza, Irba and Kaz deposits; the weakest properties characterize the lightly oxidized ore from Izykh-Gol and Krasnokamensk; the magnetic characteristics are proportional to magnetite content in a primary test specimen. Considering this, the integrated processing of lightly oxidized and magnetite ore is recommended to lower magnetite loss in tailings of Abagur plant.

WoS,
Смотреть статью,
WOS,
Для получение полного текста обратитесь в библиотеку

Держатели документа:
Russian Acad Sci, Siberian Branch, LV Kirensky Phys Inst, Krasnoyarsk 660036, Russia
EVRAZRUDA JSC, Novokuznetsk 654027, Russia

Доп.точки доступа:
Yakubailik, E. K.; Якубайлик, Эдуард Константинович; Kilin, V. I.; Килин, В. И.; Chizhik, M. V.; Чижик, Михаил Владимирович; Ganzhenko, I. M.

    Изучение обогатимости гематит-магнетитовых руд Абагасского месторождения
/ В. И. Килин [и др.] // Физ.-техн. проблемы разраб. полез. ископаемых. - 2012. - № 2. - С. 160-166. - Библиогр.: 3 назв. . - ISSN 0015-3273
Аннотация: Различными методами магнитной сепарации исследована обогатимость двух основных типов руд Абагасского железорудного месторождения: гематито-магнетитового и магнетито-мушкетовитового. Сухой магнитной сепарацией достигнуты приемлемые для первой стадии показатели обогащения, а мокрой - выделены высококачественные железорудные концентраты. На смешанных гематит-магнетитовых рудах опробована двухстадиальная схема обогащения, значительно повысившая суммарное извлечение железа из руды.

РИНЦ,
Для получение полного текста обратитесь в библиотеку

Держатели документа:
Институт физики им. Л.В. Киренского СО РАН

Доп.точки доступа:
Килин, В. И.; Kilin, V. I.; Якубайлик, Эдуард Константинович; Yakubailik E. K.; Костененко, Лариса Павловна; Ганженко, И. М.

    Магнитные характеристики первичных концентратов руд – сырья Абагурской фабрики
/ Э. К. Якубайлик [и др.] // Физ.-техн. проблемы разраб. полез. ископаемых. - 2013. - № 1. - С. 170-176 . - ISSN 0015-3273
   Перевод заглавия: Magnetic characteristics of primary concentrates supplied as a feedstock to abagur enrichment-agglomeration plant
Аннотация: Работа содержит результаты измерений основных магнитных характеристик девяти первичных концентратов магнетитовых и слабоокисленных руд железорудных месторождений Сибири — сырья Абагурской фабрики. Наибольшими значениями магнитных параметров обладают магнетитовые промпродукты Абазы, Ирбы, Каза; наименьшими — слабоокисленные Изых-Гола, Краснокаменска; значения характеристик пропорциональны содержанию магнетита в исходной пробе. Учитывая это, слабоокисленные руды необходимо обогащать совместно с магнетитовыми для снижения потерь магнетита в хвосты.

Смотреть статью,
Для получение полного текста обратитесь в библиотеку

Держатели документа:
Институт физики им. Л.В. Киренского СО РАН

Доп.точки доступа:
Якубайлик, Эдуард Константинович; Yakubailik, E. K.; Килин, В. И.; Kilin, V. I.; Чижик, Михаил Владимирович; Chizhik, M. V.; Ганженко, И. М.; Килин, С. В.; Kilin, S. V.

    Магнитные свойства и процессы мокрой магнитной сепарации первичных концентратов железосодержащих руд Сибири
/ Э. К. Якубайлик [и др.] // Горный информационно-аналитический бюллетень. - 2013. - № 2. - С. 114-124 . - ISSN 0236-1493
   Перевод заглавия: Magnetic properties and process wet separation of the primary concentrate iron ores Siberia
Аннотация: Изложены результаты изучения основных магнитных характеристик и показателей лабораторной мокрой сепарации девяти первичных концентратов магнетитовых и слабоокисленных руд сибирских месторождений — сырья Абагурской обогатительной фабрики. Рекомендовано слабоокисленные руды обогащать в обшей шихте с магнетитовыми для уменьшения потерь железа с хвостами.
The results of investigation of the main magnetic properties and the separation parameters obtained laboratory wet separation nine primary concentrate magnetite and sub-acidulute siberian ores deposits - raw materials of Abagursk preparation plant are present. Recommend sub-acidulate ores to concentrate at common charge with the magnetite ores for decreasing the losses of the iron with tailing.

Смотреть статью,
Для получение полного текста обратитесь в библиотеку

Держатели документа:
Институт физики СО РАН
ОАО «Евразруда»
ЗАО «Полюс»

Доп.точки доступа:
Якубайлик, Эдуард Константинович; Yakubailik, E. K.; Килин, В. И.; Kilin, V. I.; Килин, С. В.; Kilin, S. V.; Ганженко, И. М.

    Цифровая фотография – оперативный метод исследования процессов магнитной сепарации сильномагнитных руд
/ В. И. Килин, Э. К. Якубайлик, С. В. Килин // Горный информационно-аналитический бюллетень. - 2013. - № 11. - С. 130-136
   Перевод заглавия: The digital photo technique - routine method investigation process magnetic separation strong-magnetic ores
Аннотация: Приведены результаты изучения процессов намагничивания (флокуляции) и размагничивания (дефлокуляции) сильномагнитных продуктов Абагурской обогатительной фабрики методом цифровой фотографии. Наблюдалась как «наведенная» внешним полем флокуляция, так и «остаточная» – за счет остаточной намагниченности. Поле в 40 кА/м. можно считать оптимальным как для намагничивания, так и для размагничивания сильномагнитных продуктов.
The results investigation process magnetization (flocculation) and demagnetization (deflocculation) Abagurskoy manufacture products by digital photo technique are presented. It was observer both flocculation induced by external field, and it,s own due to remanent magnetization. Field value equals to 40 kA/m can be considered optimal both for magnetization and for demagnetization of products.

Смотреть статью,
Для получение полного текста обратитесь в библиотеку

Держатели документа:
Институт физики им. Л.В. Киренского СО РАН

Доп.точки доступа:
Якубайлик, Эдуард Константинович; Yakubailik, E. K.; Килин, С. В.; Kilin, S. V.; Kilin V. I.

    Изучение процессов намагничивания и размагничивания сильномагнитных руд методом цифровой фотографии
/ Э. К. Якубайлик [и др.] // Изв. вузов. Черная металлургия. - 2013. - № 2. - С. 5-11 . - ISSN 0363-0797
Аннотация: Содержатся результаты изучения процессов намагничивания (флокуляции) и размагничивания (дефлокуляции) продуктов Абагурской обогатительно-агломерационной фабрики методом цифровой фотографии. Наблюдались как «наведенная» внешним полем флокуляция, так и «собственная» за счет остаточной намагниченности; процесс размагничивания за счет собственной флокуляции. Интервал постоянных полей намагничивания от 24 до 200 кА/м. Напряженность переменного поля в процессе дефлокуляции от 6 до 40 кА/м, пробы намагничивались при 48 кА/м. Формы флокул, образующихся в магнитном поле и за счет остаточной намагниченности, различны. Сущест венных отличий во флокуляции и дефлокуляции разных абагурских продуктов не обнаружено. Поля напряженностью 40 кА/м можно считать оптимальными как для намагничивания, так и для размагничивания продуктов. Такие параметры поля (постоянного и переменного) технически достижимы на фабрике.
Processes of magnetization (flocculation) and demagnetization (deflocculation) of products of Abagurskaya concentrating-sintering factory were investigated by digital photo technique. Both induced by the ‘external’ field flocculation and ‘own’ flocculation due to the remanent magnetization were observed as well as demagnetization process of ‘own’ flocculation. Interval of constant fields of magnetization is from 24 to 200 kA / m. The flocculi forms formed in the magnetic field due to remanent magnetization are different. No significant differences in flocculation and defl occulation of various factory’s products were found. The fields of 40 kA intensity might be considered optimal for magnetization and demagnetization of products. Such fields (constant and alternating) are technically possible at the factory.

РИНЦ

Держатели документа:
Институт физики им. Л.В. Киренского СО РАН

Доп.точки доступа:
Якубайлик, Эдуард Константинович; Yakubailik, E. K.; Килин, В. И.; Kilin, V. I.; Чижик, Михаил Владимирович; Chizhik, M. V.; Ганженко, И. М.; Килин, С. В.; Kilin, S. V.

    Dressability of abagas hematite-magnetite ores
/ V. I. Kilin [et al.] // J. Min. Sci. - 2012. - Vol. 48, Is. 2. - P. 363-368, DOI 10.1134/S1062739148020189. - Cited References: 3 . - ISSN 1062-7391

Кл.слова (ненормированные):
magnetite -- hematite -- ilvaite -- dry -- wet -- high-gradient magnetic separation -- jigging

Аннотация: A number of magnetic separation processes are used to study preparability of two main hematite-magnetite and magnetite-muscovite ore types extacted it the Abagas iron ore deposit. The dry magnetic separation results were judged as acceptable for the rough processing stage, while the products of the wet magnetic separation were the high-grade iron ore concentrates. The two-stage beneficiation tests on complex hematite-magnetite ores demonstrated much higher cumulative iron recovery from the test ore.

Смотреть статью,
Scopus,
WoS,
Для получение полного текста обратитесь в библиотеку

Держатели документа:
[Kilin, V. I.] EVRAZRUDA, Novokuznetsk 654027, Russia
[Yakubailik, E. K.
Kostenenko, L. P.] Russian Acad Sci, LV Kirensky Phys Inst, Siberian Branch, Krasnoyarsk 660036, Russia
[Ganzhenko, I. M.] Siberian Fed Univ, Krasnoyarsk 660041, Russia

Доп.точки доступа:
Kilin, V. I.; Килин, В. И.; Yakubailik, E. K.; Якубайлик, Эдуард Константинович; Kostenenko, L. P.; Костененко, Лариса Павловна; Ganzhenko, I. M.

    Wet magnetic separation of Siberian iron-ore concentrates
/ E. K. Yakubailik [et al.] // Steel Transl. - 2014. - Vol. 44, Is. 2. - P. 113-116, DOI 10.3103/S096709121402020X. - Cited References: 3 . - ISSN 0967-0912. - ISSN 1935-0988

Кл.слова (ненормированные):
concentrate -- ore -- wet magnetic separation

Аннотация: Wet separation of the primary Siberian iron-ore concentrates processed at Abagursk enrichment facility (OAO Evrazruda) is studied in the laboratory. Nine samples of concentrates (-0.07 mm class) from magnetite ore and weakly oxidized ore are subjected to wet magnetic analysis in a field of 80 kA/m. The basic magnetic characteristics of the initial concentrates and the products obtained on separation are measured. The yield of magnetic product is greatest for magnetite ores: more than 68% (Abakan), as compared to 43-45% for weakly oxidized ore. Thus, the yield of magnetic product falls with decrease in magnetite content in the initial material. The following practical recommendations are offered: (1) it is expedient to enrich weakly oxidized ore after mixing with magnetite ore, so as to reduce the loss of iron with the tailings; (2) the magnetic systems of PBM 90/250 separators must be reconstructed, with the introduction of stronger magnets. © 2014 Allerton Press, Inc.

Смотреть статью,
Scopus,
Для получение полного текста обратитесь в библиотеку

Держатели документа:
Institute of Physics, Siberian Branch, Russian Academy of Sciences, Krasnoyarsk, Russian Federation
OAO Evrazruda, Novokuznetsk, Russian Federation
OAO Krastsvetmet, Krasnoyarsk, Russian Federation
ZAO Polyus, Krasnoyarsk, Russian Federation

Доп.точки доступа:
Yakubailik, E. K.; Якубайлик, Эдуард Константинович; Kilin, V. I.; Килин, В. И.; Ganzhenko, I. M.; Chizhik, M. V.; Чижик, Михаил Владимирович; Kilin, S. V.; Килин, С. В.

    Лабораторные исследования мокрой магнитной сепарации первичных концентратов сибирских железорудных месторождений
/ Э. К. Якубайлик [и др.] // Изв. вузов. Чер. металлургия. - 2014. - № 2. - С. 47-51. - Библиогр.: 3 назв. . - ISSN 0363-0797
ГРНТИ

Кл.слова (ненормированные):
мокрая магнитная сепарация -- концентрат -- руда

Аннотация: Подведены результаты исследований лабораторной мокрой сепарации первичных концентратов железорудных месторождений Сибири - сырья Абагурской обогатительной фабрики ОАО "Евразруда". Мокрый магнитный анализ выполнен на девяти пробах класса -0,07 мм промпродуктов двух типов руд - магнетитовых и слабоокисленных в магнитном поле 80 кА/м. Измерены основные магнитные характеристики исходных первичных концентратов и продуктов их сепарации. Наибольший выход магнитного продукта получен на магнетитовых рудах - более 68% (Абакан), на слабоокисленных - существенно меньше (43-45%), т. е. выход падает с уменьшением содержания магнетита в исходном материале. Практические рекомендации: слабоокисленные руды целесообразно обогащать в общей шихте с магнетитовыми для уменьшения потерь железа с хвостами; необходимо завершить реконструкцию магнитных систем сепараторов ПБМ 90/250 с переходом на высокоинтенсивные магниты

Смотреть статью в номере журнала,
РИНЦ

Держатели документа:
Институт физики им. Л.В. Киренского СО РАН

Доп.точки доступа:
Якубайлик, Эдуард Константинович; Yakubailik, E. K.; Килин, В. И.; Kilin, V. I.; Ганженко, И. М.; Чижик, Михаил Владимирович; Chizhik, M. V.; Килин, С. В.; Kilin, S. V.

    Уровень потерь магнетитового железа при мокрой сепарации
/ Э. К. Якубайлик [и др.] // Изв. вузов. Черн. металлургия. - 2016. - Т. 59, № 6. - С. 397-401, DOI 10.17073/0368-0797-2016-6-397-401. - Библиогр.: 15 . - ISSN 0368-0797
Аннотация: Изучены пробы отвальных хвостов всех операций, проводимых по схеме обогащения Абагурской фабрики. Выполнены магнитный, химический анализы общих хвостов, измерены магнитные характеристики продуктов. Среднее содержание железа магнетитового в отвальных хвостах составило в 2013 г. примерно 0,9 %. Опыты подтвердили, что основные потери магнетита связаны с его тонкими классами, их низкими магнитными параметрами. Потери магнетита снижаются с повышением поля сепарации. На фабрике заменено45 % феррит-бариевых магнитных систем сепараторов ПБМ 90/250 на системы из композитов неодим - железо - бор; поле возросло с 111 до 175 кА/м. Рекомендовано завершить модернизацию магнитных систем всех сепараторов фабрики; на операции сгущения установить сепараторы для регенерации суспензий с полем 190 кА/м. В итоге реконструкции уровень потерь магнетитового железа на фабрике может быть достигнут 0,45 - 0,55 %.

Смотреть статью,
РИНЦ,
Для получение полного текста обратитесь в библиотеку

Держатели документа:
ЗАО «ГМК Казахалтын»
Институт физики СО РАН им. Л.В. Киренского
ОАО «Евразруда»

Доп.точки доступа:
Якубайлик, Эдуард Константинович; Yakubailik, E. K.; Ганженко, И. М.; Ganzhenko I. M.; Бутов, Павел Юрьевич; Butov P. Yu.; Килин, В. И.; Kilin V. I.
669.046
О-93

    ОЦЕНКА ОБОГАТИМОСТИ АБАГАЗСКИХ ОКИСЛЕННЫХ РУД
[Текст] / В. И. Килин [и др.] // Известия высших учебных заведений. Черная металлургия. - 2011. - № 12. - С. 6-8 . - ISSN 0368-0797. - ISSN 2410-2091
ГРНТИ
УДК
Рубрики:


РИНЦ

Держатели документа:
Институт физики СО РАН
ОАО «Евразруда»
Сибирский федеральный университет

Доп.точки доступа:
Килин, В.И.; Якубайлик, Э.К.; Ганженко, И.М.; Килин, С.В.