    In vivo study of 2D PHA matrices of different chemical compositions: tissue reactions and biodegradations [Text] / T. G. Volova [et al.] // Mater. Sci. Technol. - 2014. - Vol. 30, Is. 5. - P549-557, DOI 10.1179/1743284713Y.0000000470. - Cited References: 31. - The study was supported by the project initiated by the Government of the Russian Federation (decree no. 220 of 09.04.2010) for governmental support of scientific research conducted under the guidance of leading scientists at Russian institutions of higher learning (agreement no. 11.G34.31.0013) and the Program of Integrated Research of the Presidium of SB RAS (project no. 96). . - ISSN 0267-0836. - ISSN 1743-2847
РУБ Materials Science, Multidisciplinary + Metallurgy & Metallurgical Engineering
Рубрики:
BIOMEDICAL INVESTIGATIONS
   POLYHYDROXYALKANOATES

   VITRO

   BIOCOMPATIBILITY

   DEGRADATION

   SCAFFOLDS

   CONDUITS

   POLYMERS

Кл.слова (ненормированные):
PHA -- Polyhydroxyalkanoates -- Biocompatibility -- Implantation -- Tissue response -- Biodegradation
Аннотация: Matrices based on resorbable polyhydroxyalkanoates (PHAs) of five types {a homopolymer of 3-hydroxybutyric acid, copolymers of 3-hydroxybutyric and 4-hydroxybutyric acids [P(3HB/4HB)], 3-hydroxybutyric and 3-hydroxyvaleric acids [P(3HB/3HV)], 3-hydroxybutyric and 3-hydroxyhexanoic acids [P(3HB/3HHx)]} have been constructed and characterised. No significant differences have been found in tissue response to implantation of these PHAs. Non-coarse fibrous capsules that formed around PHA matrices reached their maximum thickness (60-90 mm) 90 days after implantation; by day 180, the average thickness of the capsules had decreased by 1.5- 2.3 times. The number of foreign body giant cells, resorbing PHAs, remained high. In vivo biodegradation behaviour of polymer matrices is related to the chemical composition of the PHA. Matrices prepared from copolymers P(3HB/4HB) and P(3HB/3HHx) exhibited the fastest degradation rates. P3HB/3HV matrices were degraded more slowly, and P3HB matrices were the most durable. In the PHA matrices that were degraded more slowly, giant cell reaction developed later.

WOS
Держатели документа:
[Volova, T. G.
Shishatskaya, E. I.
Nikolaeva, E. D.] Inst Biophys SB RAS, Krasnoyarsk 660036, Russia
[Volova, T. G.
Shishatskaya, E. I.
Nikolaeva, E. D.] Siberian Fed Univ, Inst Modern Biol & Biotechnol, Krasnoyarsk 660041, Russia
[Sinskey, A. J.] MIT, Dept Biol, Cambridge, MA 02139 USA
[Sinskey, A. J.] MIT, Engn Syst Div, Cambridge, MA 02139 USA
[Sinskey, A. J.] MIT, Hlth Sci Technol Div, Cambridge, MA 02139 USA
ИБФ СО РАН : 660036, Красноярск, Академгородок, д. 50, стр. 50

Доп.точки доступа:
Volova, T.G.; Shishatskaya, E.I.; Nikolaeva, E.D.; Sinskey, A.J.; Government of the Russian Federation

Найти похожие
 

Другие библиотеки

© Международная Ассоциация пользователей и разработчиков электронных библиотек и новых информационных технологий
(Ассоциация ЭБНИТ)